whats the best procedure for a EN16, (not T) forging, looking at the TWI its 250C preheat, basic electrodes, and slow cooling...
My thoughts were preheat, 7016 root, 7018 stringers to fillet size then a slow covered cool ??? is this best..
Also is there a route to avoid the need for preheat?